Polymer Property : Izod Impact, Unnotched (ISO) = 56.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 118 kJ/m²
56.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant
Izod Impact, Unnotched (ISO) 118 kJ/m²
56.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC (Asia Pacific)
LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 118 kJ/m²
56.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU
LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity.
Izod Impact, Unnotched (ISO) 118 kJ/m²
56.1 ft-lb/in²
ISO 180/1eU
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade)
Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio..