Polymer Property : Izod Impact, Unnotched (ISO) = 46.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 15.0 - 98.0 kJ/m²
7.14 - 46.6 ft-lb/in²
Average value: 56.2 kJ/m² Grade Count:10
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..