Polymer Property : Izod Impact, Unnotched (ISO) = 4.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP OL003A PPS - Branched
LNP* LUBRICOMP* OL003A is a compound based on PPS - Branched resin containing 15% PTFE. Added features of this grade are: Wear Resistant.
Izod Impact, Unnotched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ASTM D256
Tipco Tipcolite® THD 111 Phenolic Compound, Short Glass Fibers & Minerals, Medium -Soft Flow & High Strength
Medium -Soft Flow Phenolic Compound, Reinforced with Short Glass Fibres & MineralsApplications: Automotives & ElectricalProcessing: Compression & TransferInformation provided by the Manufacturer, T..
Izod Impact, Unnotched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON ME006 PP
LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.