Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 692 kJ/m² | 329 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 692 kJ/m² | 329 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated. |