Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 12.2 - 65.0 kJ/m² | 5.81 - 30.9 ft-lb/in² | Average value: 47.5 kJ/m² Grade Count:35 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Unnotched (ISO) | 22.0 - 65.0 kJ/m² | 10.5 - 30.9 ft-lb/in² | Average value: 39.9 kJ/m² Grade Count:23 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched (ISO) | 40.0 - 65.0 kJ/m² | 19.0 - 30.9 ft-lb/in² | Average value: 56.0 kJ/m² Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 27.0 - 65.0 kJ/m² | 12.8 - 30.9 ft-lb/in² | Average value: 39.0 kJ/m² Grade Count:8 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |