Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 42.0 - 42.0 kJ/m² @Temperature -30.0 - -30.0 °C |
20.0 - 20.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 42.0 kJ/m² Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 27.0 - 42.0 kJ/m² @Temperature -20.0 - -20.0 °C |
12.8 - 20.0 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 34.5 kJ/m² Grade Count:2 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |