Polymer Property : Izod Impact, Unnotched (ISO) = 18.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 38.0 - 38.0 kJ/m²

@Temperature -30.0 - -30.0 °C
18.1 - 18.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 38.0 kJ/m² Grade Count:1
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..