Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU (Asia Pacific) LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA6.12 LNP* LUBRICOMP* IAL12 is a compound based on Nylon 6/12 resin containing 5% PTFE, 10% Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East) LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP OX88533 PPS LNP LUBRICOMP* OX88533 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UX96507 PPA LNP* LUBRICOMP* UX96507 is a compound based on PPA containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature -30.0 °C |
18.1 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF0039S PA 66 LNP THERMOCOMP* RF0039S is a compound based on Nylon 66 resin containing 15% Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RFB33 PA6.6 (Europe-Africa-Middle East) LNP*THERMOCOMP* RFB33 is a compound based on PA66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DE003M PC LNP* STAT-KON* DE003M is a compound based on Polycarbonate containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4340 PBT 20% GF Super High Flow PBT |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp RFB53SUZ PA 66 LNP THERMOCOMP* RFB53SUZ is a compound based on Nylon 66 resin containing Glass Bead, Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WF008 PBT LNP THERMOCOMP* WF008 is a compound based on PBT resin containing 40% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Star L PA66 30V D31 PA66, Glass Fiber Filled, Injection Molded Star L PA66 30V D31 is a Molybdenum Disulfide Lubricated, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | ASTM D256 |
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² | 18.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 38.0 - 38.0 kJ/m² @Temperature -30.0 - -30.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 38.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 38.0 kJ/m² @Temperature 23.0 °C |
18.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp GL004 PSU LNP* Lubricomp* GL004 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas re.. |