Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 16.8 kJ/m² | 7.99 ft-lb/in² | ISO 180 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |