Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 26.4 kJ/m²
12.6 ft-lb/in²
ISO 180
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..