Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 115 kJ/m² | 54.7 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 115 kJ/m² | 54.7 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PX06012 PA6, Flame Retardant, Injection Molded Starflam PX06012 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |