Polymer Property : Izod Impact, Unnotched (ISO) = 1.19 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 2.50 kJ/m²

@Temperature 23.0 °C
1.19 ft-lb/in²

@Temperature 73.4 °F
ISO 180/U
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Izod Impact, Unnotched (ISO) >= 2.50 kJ/m²
>= 1.19 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet
Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe.
Izod Impact, Unnotched (ISO) 2.50 kJ/m² - NB
1.19 ft-lb/in² - NB
Average value: 48.0 kJ/m² Grade Count:19
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..