Polymer Property : Adhesive Bond Strength = 5700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 39.3 MPa

@Temperature -55.0 °C
5700 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9330.3 Paste Adhesive System
Non-slump, thixotropic adhesive with high peel strength and excellent environmental durability.Applications:Structural Repair Composite Bonding