Henkel Hysol EA 9330.3 Paste Adhesive System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9330.3 Paste Adhesive System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-slump, thixotropic adhesive with high peel strength and excellent environmental durability.Applications:Structural Repair Composite Bonding
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 42.1 MPa
6110 psi
Elongation at Break 9.0 %
9.0 %
Tensile Modulus 2.68 GPa
389 ksi
Adhesive Bond Strength 5.20 MPa

@Temperature 93.0 °C
754 psi

@Temperature 199 °F
Tensile Lap Shear
33.8 MPa

@Temperature 25.0 °C
4900 psi

@Temperature 77.0 °F
Tensile Lap Shear
39.3 MPa

@Temperature -55.0 °C
5700 psi

@Temperature -67.0 °F
Tensile Lap Shear
Peel Strength 10.6 kN/m
60.5 pli
Bell Peel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 82.0 °C
1.00 hour

@Temperature 180 °F
7200 - 10100 min

@Temperature 25.0 °C
120 - 168 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:33
Peel Strength High