Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 26.2 MPa @Temperature -55.0 °C |
3800 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol PL 7000 Film Adhesive Epoxy film adhesive formulated to provide excellent performance properties in composite bonding, and has excellent results on composite surfaces that have been exposed to bond shop environments and .. |