Polymer Property : Adhesive Bond Strength = 12.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 12.4 MPa

@Temperature 177 °C
1800 psi

@Temperature 351 °F
Lap Shear
Henkel Hysol PL 780-1 Film Adhesive
Nonmetallic, toughened, modified epoxy film designed for bonding metal, composite and thermoplastic structures. High shear properties at 350°F / 177°C. Excellent hot-wet properties. High flow ..
Adhesive Bond Strength 12.4 MPa

@Temperature 100 °C
1800 psi

@Temperature 212 °F
Lap Shear Strength vs. Aluminum
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Adhesive Bond Strength 12.4 MPa

@Temperature -55.0 °C
1800 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 956 Paste Adhesive System
Very low viscosity, cures at room temperatureDesigned for wet lay-up repairApplications: Structural Repair Low Viscosity Wet Lay-Up