Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories APM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM_36 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-35 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-38 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-39 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-40 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 500 °C, Time 10800 sec |
284.6 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories BM-2W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 500 °C, Time 10800 sec |
284.6 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories BM-3W High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories GM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MSM-36 High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MSM-38 High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MSM-39 High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories MSM-40 High-Adhesion Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SCH-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories SSM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 500 °C, Time 10800 sec |
284.6 psi @Temperature 932 °F, Time 3.00 hour |
|
Chosun Refractories SSM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ZM-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ASM-37 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 1.962 MPa @Temperature 110 °C, Time 86400 sec |
284.6 psi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories ZM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |