Mechanical Properties Metric English Comments
Charpy Impact Unnotched 9.30 J/cm²

@Temperature -20.0 °C
44.3 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 66 MI LS PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Charpy Impact Unnotched 9.30 J/cm²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66  (Unverified Data**)
Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 9.30 J/cm²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 136F6Q32 Nylon 6, 30% Glass Fiber
SAXAMID 136F6Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 30% glass fibers . Beside the high impact strength at low temperatures this grade shows very good proce..
Charpy Impact Unnotched 9.30 J/cm²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F8 Nylon 6.6, 40% Glass Fiber
SAXAMID 226F8 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 40% glass fibers. It has very high mechanical strength.Information provided by SAX Polymers
Charpy Impact Unnotched 9.30 J/cm²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
DSM Akulon® K222-KGV4 /A PA6-GF20 FR(30)
20% Glass Reinforced, Heat Stabilized, Flame Retardant (Halogen-phosphorous-free)
Charpy Impact Unnotched 9.30 J/cm²

@Temperature 23.0 °C
44.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned)
Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS ..