Polymer Property : Charpy Impact Unnotched = 6.70 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength
FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL BK039 is a 13 % glass reinforced, heat stabilized, lubricated slightly toughened black polyamide 66 for injection molding. It has improved impact resistance.Information provided by ..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eU
DSM Novamid® 1010GN8-30 NAT PA6-GF30 FR
30% Glass Reinforced, Flame Retardant, Halogen free
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont ..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, Conditioned
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Charpy Impact Unnotched 6.70 J/cm²

@Temperature -30.0 °C
31.9 ft-lb/in²

@Temperature -22.0 °F
50%RH; ISO 179/1eU
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLX BK357 is a 35% glass fiber reinforced, heat stabilized, black polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 6.70 J/cm²

@Temperature 23.0 °C
31.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Conditioned (2.5% Moisture)
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..