Polymer Property : Charpy Impact Unnotched = 26.6 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 5.60 J/cm²

@Temperature 23.0 °C
26.6 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S RV200 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact Unnotched 5.60 J/cm²

@Temperature 23.0 °C
26.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXAMID 226F5RY01 Nylon 6.6, 25% Glass Fiber
SAXAMID 226F5RY01 is a polyamide 6.6 injection-molding-grade reinforced with 25% glass fibers. It has a halogen-free flame retardant and UL listed.Information provided by SAX Polymers
Charpy Impact Unnotched 5.60 J/cm²

@Temperature 23.0 °C
26.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Charpy Impact Unnotched 5.60 J/cm²

@Temperature 23.0 °C
26.6 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, Conditioned
Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl..