Mechanical Properties Metric English Comments
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such ..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 23.0 °C
95.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® AC 30 000000 Nylon 66
PA 66, injection molding-grade, non-reinforced, higher notched impact strength than A 30 / A 31 in the dry and conditioned stateApplication Examples: plug connectors, cable binders, cable clips, par..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1501 000000 PBT
PBT, non-reinforced, injection molding, extrusion, food contact
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 23.0 °C
95.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Lanxess Pocan® KU 2-7003 000000 PBT
PBT, non-reinforced, injection molding
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179-1eU
Lanxess Pocan® B 1701 000000 PBT
PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS.
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 23.0 °C
95.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S 757 R Colored ASA
Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® E 3120 BM POM
Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
BASF Ultraform® N2320 006 POM
Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 23.0 °C
95.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
BASF Ultraform® W2320 U035 LEV POM
Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 20.0 °C
95.2 ft-lb/in²

@Temperature 68.0 °F
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy
Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness ..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 400 °C
95.2 ft-lb/in²

@Temperature 752 °F
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy
Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness ..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature 600 °C
95.2 ft-lb/in²

@Temperature 1110 °F
Kennametal Stellite Nucalloy® 430 High-Silicon Nickel-Base Hardfacing Alloy
Applications include components of chemical processing.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinations of hardness ..
Charpy Impact Unnotched 20.0 J/cm²

@Temperature -30.0 °C
95.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Lanxess Pocan® B 1600 000000 PBT
PBT, non-reinforced, injection molding, extrusion, food contact