Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 33.0 J/cm² @Temperature 23.0 °C |
157 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |