Polymer Property : Tensile Stress = 40.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber
Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® 80-7695 Polyacetal-copolymer, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Tensile Stress 40.0 MPa
5800 psi
At break; ISO 527
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Tensile Stress 40.0 MPa
5800 psi
Lehmann & Voss LUVOCOM® TPE-0900 VP Thermoplastic elastomer, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
Tensile Stress 40.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
5800 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Tensile Stress 40.0 MPa
5800 psi
Akro-Plastic Akromid® A3 4 S1 PA, Cold-Impact Resistant  (discontinued **)
The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio..