Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 1850-7795 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 65-8452-2 PP-copolymer, with carbon fiber, aramid reinforcement, lubricant modified Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Information provided by.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 80/TF/18/SI/2/BK Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® 80-7695 Polyacetal-copolymer, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | At break; ISO 527 |
FKuR Kunststoff Bio-Flex® F 6513 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Lehmann & Voss LUVOCOM® TPE-0900 VP Thermoplastic elastomer, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Tensile Stress | 40.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
5800 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Tensile Stress | 40.0 MPa | 5800 psi | |
Akro-Plastic Akromid® A3 4 S1 PA, Cold-Impact Resistant
(discontinued **) The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilizatio.. |