Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.30 MPa @Strain 100 % |
334 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-65B200 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to thermoset EPDM rubber .. |
|||
Tensile Stress | 2.30 MPa @Strain 100 % |
334 psi @Strain 100 % |
Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories.. |