Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 25.0 MPa | 3630 psi | |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Tensile Stress | 25.0 MPa | 3630 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
Tensile Stress | 25.0 MPa | 3630 psi | ISO R527 |
Iran Petrochemical (PCC) EP2C 37 F Polypropylene EP2S 37 F offers good process ability, excellent clarity and gloss and exhibits very good heat weld ability.Applications: packaging of stationery, packaging of food stuffs, lamination.Information pr.. |
|||
Tensile Stress | 25.0 MPa | 3630 psi | ISO R527 |
Iran Petrochemical (PCC) EP2S 30 B Polypropylene This is a medium modified PP random copolymer. The product is designed for the extrusion of film and sheet and for blow molding small and medium sized item.Applications: Packaging of cosmetics, d.. |
|||
Tensile Stress | 25.0 MPa | 3630 psi | |
Lehmann & Voss LUVOCOM® 100-7846 Thermoplastic polyurethane, with aramid reinforcement Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Tensile Stress | 25.0 MPa @Strain 50.0 % |
3630 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |