Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.7 MPa | 2420 psi | at Break, MD; ASTM D882 |
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria.. |