Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 14.7 MPa @Strain 100 % |
2130 psi @Strain 100 % |
ASTM D412 |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |