Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 94.8 MPa | 13700 psi | ASTM D3759 |
3M 399FR Flame Retardant Glass Cloth Tape 3M™ Flame Retardant Glass Cloth Tape 399FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typic.. |