Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 94.5 MPa | 13700 psi | ASTM D638 |
Chase Plastics CP Pryme® NN133GTL (COND, 50% RH) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Tensile Strength at Break | 94.8 MPa | 13700 psi | ASTM D3759 |
3M 399FR Flame Retardant Glass Cloth Tape 3M™ Flame Retardant Glass Cloth Tape 399FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typic.. |