Polymer Property : Tensile Strength at Break = 914 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.30 MPa
914 psi
ISO 37
PolyOne OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Strength at Break 6.30 MPa
914 psi
ISO 37
ELASTO UK Dryflex® 3039-201 TPE, Modified Injection Molding Grade for Sanitary Seals
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3039-201 is specifically designe..