Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.30 MPa | 914 psi | ISO 37 |
PolyOne OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Strength at Break | 6.30 MPa | 914 psi | ISO 37 |
ELASTO UK Dryflex® 3039-201 TPE, Modified Injection Molding Grade for Sanitary Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3039-201 is specifically designe.. |