Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 91.7 MPa | 13300 psi | |
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |