Polymer Property : Tensile Strength at Break = 8800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.7 MPa
8800 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Tensile Strength at Break 60.7 MPa
8800 psi
ASTM D638
Niche Polymer PPCG20BK Copolymer PP, 20% Glass Fiber Filled
Information provided by Niche Polymer
Tensile Strength at Break 60.7 MPa
8800 psi
2 in/min; ASTM D638
RheTech Products F25-01 34% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Support ductsHousingsBattery traysArm rest insertsInjection molding conditions reported in table.Information provided by RheTech Products.
Tensile Strength at Break 60.7 MPa
8800 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding ..
Tensile Strength at Break 60.7 MPa
8800 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL..
Tensile Strength at Break 60.7 MPa
8800 psi
ASTM D638
Chase Plastics CP Pryme® NN200L (COND, 50% RH) Nylon 66, Internally Lubricated
Information provided by Chase Plastics.
Tensile Strength at Break 60.7 MPa
8800 psi
2 in/min; ASTM D638
RheTech Products G20P252-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Natural
Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products.