Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 86.1 MPa | 12500 psi | ASTM D638 |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |