Polymer Property : Tensile Strength at Break = 856 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.90 MPa
856 psi
ASTM D412
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness
KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber ..
Tensile Strength at Break 5.90 MPa
856 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Tensile Strength at Break 5.90 MPa
856 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio..
Tensile Strength at Break 5.90 MPa
856 psi
ASTM D638 - ISO 527-2
DuPont Elvaloy® 741 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont.
Tensile Strength at Break 5.90 MPa
856 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate
Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app..
Tensile Strength at Break 5.90 MPa
856 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Tensile Strength at Break 5.90 MPa
856 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
Tensile Strength at Break 5.90 MPa
856 psi
ISO 37
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 5.90 MPa
856 psi
ISO 37
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..