Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.90 MPa | 855 psi | 158°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 8291-85PA Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/s.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | ASTM D412 |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4175 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4175 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 4475 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4475 is a medium hardness grade possessing exceptional tensile strength, superior compressio.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | ASTM D638 - ISO 527-2 |
DuPont Elvaloy® 741 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 291-60B150 Thermoplastic Vulcanizate Product Description: A colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PC, ABS, PC/ABS, ASA and PMMA for app.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | ISO 37 |
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 5.90 MPa | 856 psi | ISO 37 |
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 5.90 MPa | 855 psi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ DGR 6150 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6150 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6,
Nylon 6/6, glass filled Nylo.. |