Mechanical Properties Metric English Comments
Tensile Strength at Break 8.48 MPa
1230 psi
510 mm/min; ASTM D412A
PolyOne Geon™ Vinyl Flexible XV3715 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength at Break 8.48 MPa
1230 psi
Across flow; ASTM D412
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic elastomer with good fluid resistance, formulated to replace foamed thermoset elastomers such as EPDM and thermoplastic foams. It is polyolefin-based and desig..
Tensile Strength at Break 8.48 MPa
1230 psi
Crosshead Speed - 20 in/min; ASTM D638
LyondellBasell Petrothene® NA860008 Low Density Polyethylene
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel..
Tensile Strength at Break 8.48 MPa
1230 psi
Crosshead Speed - 20 in/min; ASTM D638
LyondellBasell Petrothene® NA860241 Low Density Polyethylene
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel..
Tensile Strength at Break 8.48 MPa
1230 psi
ASTM D412
Teknor Apex Monprene® MP-1852A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 8.48 MPa
1230 psi
ASTM D412
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 8.48 MPa
1230 psi
ASTM D412
Teknor Apex Telcar® TL-2585F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 8.48 MPa
1230 psi
ASTM D 412
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tensile Strength at Break 8.48 MPa
1230 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8223-30M300 Thermoplastic Elastomer
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and ..
Tensile Strength at Break 8.48 MPa
1230 psi
ISO 37
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 8.48 MPa
1230 psi
ISO 37
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 8.48 MPa
1230 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-73W175 Thermoplastic Elastomer  (discontinued **)
A soft, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for thin wall ..