Mechanical Properties Metric English Comments
Tensile Strength at Break 8.41 MPa
1220 psi
ASTM D412
Teknor Apex APEX® 1519-45 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company
Tensile Strength at Break 8.41 MPa
1220 psi
ASTM D412
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..