Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.41 MPa | 1220 psi | ASTM D412 |
Teknor Apex APEX® 1519-45 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMForms-PelletsFeatures- Good flexibility Information provided by Teknor Apex Company |
|||
Tensile Strength at Break | 8.41 MPa | 1220 psi | ASTM D412 |
Teknor Apex Telcar® TL-1934C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |