Mechanical Properties Metric English Comments
Tensile Strength at Break 49.0 - 54.0 MPa
7110 - 7830 psi
ASTM D638
Solvay Specialty Polymers solvene® 250 EAP Electroactive Polymer (EAP)
Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/..
Tensile Strength at Break 49.0 - 54.0 MPa
7110 - 7830 psi
ASTM D638
Solvay Specialty Polymers solvene® T 2808 Electroactive Polymer (EAP)
Annealing Temperature - < 135 °C; Breakdown Voltage - 250 kV/mm; Coercive Field - 50 kV/mm; Crystallization Point - ASTM D3418 123 °C; Curie Temperature - ASTM D3418 110 °C; d33 - -38.0 pC/..
Tensile Strength at Break 42.0 - 54.0 MPa
6090 - 7830 psi
5 mm/min.; IS 867-1963
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha..