Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 528 MPa | 76600 psi | 304 Stainless Steel butt joint. |
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types .. |