Polymer Property : Tensile Strength at Break = 528 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 528 MPa
76600 psi
304 Stainless Steel butt joint.
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy
Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types ..