Mechanical Properties Metric English Comments
Tensile Strength at Break 5.17 MPa

@Temperature 23.0 °C
750 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - ..
Tensile Strength at Break 5.17 MPa
750 psi
TM R050-36
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin
Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (..
Tensile Strength at Break 5.17 MPa
750 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer  (discontinued **)
A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner ..
Tensile Strength at Break 5.17 MPa
750 psi
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible H41276D Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 5.17 MPa
750 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R1211P Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D638 ISO 527-2
DuPont Elvax® 4320 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s..
Tensile Strength at Break 5.17 MPa
750 psi
Post oven cured 24 hours at 480°F
Malvern Minerals Sliastic 740 with 33% Novacite® Daper Quartz Filler
Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company.
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Monprene® MP-1277B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 5.17 MPa
750 psi
Flow; ASTM D412
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Monprene® MP-2250 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer
Uses: Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed..
Tensile Strength at Break 5.17 MPa
750 psi
ASTM D412
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 5.17 MPa
750 psi
3M VFP-876 Tubing
3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to..
Tensile Strength at Break 5.17 MPa
750 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer  (discontinued **)