Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.96 MPa | 720 psi | ASTM D412 |
Teknor Apex Telcar® TL-1522A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 4.96 MPa | 720 psi | Air at 158°F, 96 hr; ASTM D573 |
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo.. |