Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.688 MPa | 1115 psi | DCBP Cure |
Shin-Etsu Silicones KE-541U Silicone Rubber KE541U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending fill.. |