Shin-Etsu Silicones KE-541U Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones KE-541U Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KE541U is one of a series of easy processing, general purpose grade silicone rubber bases. It can be used in a variety of applications requiring finishing by molding or extruding with extending filler.Product Features: This product can be blended with KE551U, KE561U, KE571U, and KE581U for intermediate hardnesses. The choice between these bases will depend on specific requirements.Typical Applications: Roll covers.Diaphragms.O-rings and gaskets./ul>Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
DCBP Cure
1.10 g/cc
1.10 g/cc
DBPH Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
DBPH Cure
42
42
DCBP Cure
Tensile Strength at Break 7.688 MPa
1115 psi
DCBP Cure
9.86 MPa
1430 psi
DBPH Cure
Elongation at Break 460 %
460 %
DCBP Cure
730 %
730 %
DBPH Cure
100% Modulus 0.000689 GPa
0.100 ksi
DBPH Cure
0.000896 GPa
0.130 ksi
DCBP Cure
Tear Strength 1.23 kN/m
7.00 pli
Die B; DBPH Cure
13.0 kN/m
74.0 pli
Die B; DCBP Cure
Compression Set 13 %

@Temperature 150 °C,
Time 79200 sec
13 %

@Temperature 302 °F,
Time 22.0 hour
DCBP Cure
Descriptive Properties Value Comments
Cure Agent DBPH
DCBP
Cure Type Post Cure