Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 48.1 MPa | 6980 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 48.1 MPa | 6980 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0941 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 48.1 MPa | 6980 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Tensile Strength at Break | 48.1 MPa | 6980 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SC 203EL General Purpose Polystyrene CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cass.. |