Supreme Petrochem SC 203EL General Purpose Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Supreme Petrochem LTD
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Supreme Petrochem SC 203EL General Purpose Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CharacteristicsMedium flow grade with good mechanical properties Improves productivity due to good balance of flow, heat and mold release propertiesProcessing Injection moldingApplicationsAudio cassettes housing and covers Medical applications like disposable infusion trays, screw vials etc. Crystal wares, mugs, trays, bowls, pen stands, fruit bowls, service trays etc.Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640, UL file E185934Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.1 MPa
6980 psi
50 mm/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
50 mm/min; ASTM D638
Flexural Strength 80.4 MPa

@Thickness 3.20 mm
11700 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 2.84 GPa

@Thickness 3.20 mm
412 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 0.200 J/cm

@Thickness 3.20 mm
0.375 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F