Polymer Property : Tensile Strength at Break = 66.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 66.7 MPa
9670 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Tensile Strength at Break 66.7 MPa
9670 psi
ASTM D638
Unitika elitel UE3210 Polyester, Pellet
Medium Tg, standard resin, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi..
Tensile Strength at Break 66.7 MPa
9670 psi
ASTM D3759
3M 855 High Temperature Nylon Tape
3M™ High Temperature Nylon Tape 855 is a 2 mil nylon film tape with a non-silicone rubber adhesive that can be used in many composite bagging operations or to help remove flashing after composite b..
Tensile Strength at Break 66.7 MPa
9670 psi
50 mm/min; ASTM D638
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.